Biodesign/Projects/Electroactive properties of Silk
MEASURING STATIC ON SILK WITH A MAINS-POWERED OSCILLOSCOPE
Purpose Detect charging, compare patches of fabric, and watch charge decay. This setup does not measure the silk's absolute voltage or total charge.
Equipment Bench oscilloscope; 10x passive probe; small foil square (about 2 x 2 cm); insulating tape; silk; rubbing material; ruler. Optional: 1 Mohm series resistor to protect the probe input from accidental contact.
Safety and grounding A bench scope's probe ground clip and BNC shell are usually connected to protective earth. Never defeat the earth connection. Never put the ground clip on the fabric, a person, or an electrical outlet. Keep the sensing foil and probe tip away from sparks and from mains wiring. If there may be strong sparks, use a field meter instead. Do not touch the probe tip with charged fabric.
Setup 1. Tape the foil square to an insulating surface and connect the probe tip to it. If available, place a 1 Mohm resistor between foil and tip; this is a precaution against accidental discharge, not a calibrated voltage divider. 2. Clip the probe ground to the oscilloscope's ground terminal, or leave it connected to the grounded probe shield as normally supplied. Keep the ground lead away from the foil and silk. Never connect the ground clip to the sensing foil. 3. Set the channel and physical probe to 10x, DC coupling, 1 V/div initially, and about 0.5 s/div. Adjust sensitivity to keep the trace on screen. Use single acquisition or normal trigger when the signal is too brief to inspect. 4. Keep the foil fixed. Mark a point 3-5 cm in front of it so each pass of the silk uses the same distance. First move uncharged silk toward and away from the foil to observe the baseline.
Measurement 5. Rub one section of silk with your chosen material. Move that section slowly toward the sensing foil without touching it, pause briefly, then withdraw it. Save or note the trace. 6. Repeat with the same distance, angle, motion, area and rubbing procedure. Compare peak deflection and the direction of the trace against the baseline. Measure again after 10, 30 and 60 seconds to see decay. 7. For a spatial comparison, test different sections of silk at the same distance. Record temperature and relative humidity if possible; humidity can strongly affect charge persistence.
How to interpret it The foil and charged silk form a changing capacitive coupling. Moving silk usually produces a transient; a stationary piece can produce an offset that drifts because the probe input leaks charge. Deflection depends on geometry, motion, scope input and nearby grounded objects. Do not call the trace the silk's voltage, and do not infer coulombs from it. A reversed trace can suggest reversed charge polarity if every aspect of the geometry and movement stays the same, but verify polarity with a calibrated instrument.
Record sheet Date/time: ______ Ambient humidity: ______ Rubbing material and number of strokes: ______ Fabric patch: ______ Distance: ______ Delay after rubbing: ______ Scope settings: ______ Baseline peak: ______ Charged peak: ______